Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

Looking for stress corrosion cracking resistant C61300 bronze plates for marine hardware? Our factory offers high quality 1000mm plates at competitive prices.
Request a Quote

PRODUCTS DETAILS

  • Overview
  • Product Description
  • Chemical Composition
  • Products List
  • Certifications
  • Production flow
  • Packaging & Shipping
  • Company Profile
  • FAQ
Overview

Basic Info.

Model NO.
C61300
Thickness
0.1mm~120mm
Width
10mm~2000mm
Temper
Soft Anneal, Deep-Drawing Anneal, etc
Surfaces
Mill, Polished, Bright, Oiled, Hair Line,etc
Standards
ASTM, GB, ISO, DIN, BS, JIS, En, etc.
Transport Package
Bundles or as Customer′s Requirement
Trademark
ZYTC
Origin
China
HS Code
7409119000
Production Capacity
200tons/Month

Product Description

 
Product Description

Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

Product Name Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Standard ASTM, AISI, DIN, EN, GB, JIS, etc
Material ASTM B171/171M-2018: C61300
MOQ 300Kg
Package Standard export package, suited for all kinds of transport, or as required. 
price term EXW, FOB, CFR, CIF, DDP, etc.
Contact If you have any questions, please feel free to contact me. We are sure your inquiry or requirements will get prompt attention.
 
GRADE TECHNOLOGY TEMPER SPECIFICATION(MM)
THICKNESS WIDTH LENGTH
COPPER  HOT ROLLED M20 4~8 600~3100 ≤6000
>8~150 200~3100 ≤6000
COLD ROLLED O60,H01,H02,H04,H06,H08 0.3~<0.5 400~610 ≤2000
0.5~3.0 400~1020 ≤3000
>3.0~12 400~3100 ≤8000

 B171/171M-2018
This specification establishes the requirements for plates, sheets, and circles cut from plates and sheets made of UNS C36500, C44300, C44400, C44500, C46400, C46500, C61300, C61400, C63000, C63200, C70600, C70620, C71500, C71520, or C72200 copper alloy. These materials are recommended for use in pressure vessels, condensers, and heat exchangers. The materials are manufactured by either hot rolling or forging and finished by cold working and annealing to produce products of the required dimensions and properties. Tempers available under this specification are as hot rolled and hot rolled and annealed. The products manufactured for ASME Boiler and Pressure Vessel code applications must be certified to the hot rolled and annealed temper while all other products can either have hot rolled or hot rolled and annealed temper. This specification also contains information on the required material chemical compositions, densities, and tensile properties.
Chemical Composition

Chemical Composition

  Cu(%) Pb(%) Sn Zn(%) Fe(%) P As Sb
C36500 58.0~61.0 0.25~0.7 0.25 Rem 0.15      
C44300 70.0~73.0 0.07 0.8~1.2 Rem 0.06   0.02~0.06  
C44400 70.0~73.0 0.07 0.8~1.2 Rem 0.06     0.02~0.10
C44500 70.0~73.0 0.07 0.8~1.2 Rem 0.06 0.02~0.10    
C46400 59.0~62.0 0.20 0.50~1.0 Rem 0.1      
C46500 59.0~62.0 0.20 0.50~1.0 Rem 0.10   0.02~0.06  
 
  Cu Pb Sn Zn Fe P Ni Al Mn Si
C61300 Rem 0.01 0.20~0.50 0.10 2.0~3.0 0.015 0.15 6.0~7.5 0.20 0.10
C61400 Rem 0.01   0.20 1.5~3.5 0.015   6.0~8.0 1.0  
C63000 Rem   0.20 0.30 2.2~4.0   4.0~5.5 9.0~11.0 1.5 0.25
C63200 Rem 0.02     3.5~4.3   4.0~4.8 8.7~9.5 1.2~2.0 0.10
 
  Cu Pb Zn Fe P Ni C Cr Mn S Si Ti
C70600 Rem 0.05 1.0 1.0~1.8   9.0~11.0     1.0      
C70620 86.5 0.02 0.50 1.0~1.8 0.02 9.0~11.0 0.05   1.0 0.02    
C71500 Rem 0.05 1.0 0.40~1.0   29.0~33.0     1.0      
C71200 65.0 0.02 0.50 0.40~1.0 0.02 29.0~33.0 0.05   1.0 0.02    
C72200 Rem 0.05 1.0 0.50~1.0   15.0~18.0   0.30~0.7 1.0   0.03 0.03

Copper Alloy 
Type (GB) (ISO) (ASTM) (EN) (JIS) (BS) (DIN)
Red copper TU2 Cu-OF C10100 CW008A C1011 C101 OF-Cu
T2 Cu-FRHC C11000   C1100 C101 E-Cu58
TP2 Cu-DHP C12200 CW024A C1220 C106 SF-Cu
TP1 Cu-DLP C12000 CW023A C1201   SW-Cu
Sliver copper TAg0.1 CuAg0.1 C10400   C1040   CuAg0.1
Brass H90 CuZn10 C22000 CW501L C2200 CZ101 CuZn10
H70 CuZn30 C26000 CW505L C2600 CZ106 CuZn30
H68   C26200 CW506L C2620   CuZn33
H65 CuZn35 C27000 CW507L C2700 CZ107 CuZn36
H63 CuZn37 C27200 CW508L C2720 CZ108 CuZn37
H62 CuZn40 C28000 CW509L C2800 CZ109  
Tin-Bronze copper QSn4-0.3 CuSn4 C51100 CW450K C5111 PB101 CuSn4
CuSn5 C51000 CW451K C5101   CuSn5
QSn6.5-0.1 CuSn6 C51900 CW452K C5191 PB103 CuSn6
QSn8-0.3 CuSn8 C52100 CW453K C5210   CuSn8
QSn6.5-0.4            
Zn-white copper BZn18-18 CuNi18Zn20 C75200 CW409J C7521 NS106 CuNi18Zn20
BZn18-26 CuNi18Zn27 C77000 CW410J C7701 NS107 CuNi18Zn27
BZn15-20       C7541    

 
C61300

     A single phase ductile aluminium bronze with the addition of tin to give excellent corrosion resistance and low magnetic permeability.
     This alloy is ductile and can be cold worked. It is normally manufactured in the form of tube plate to be used in water condenser system, pressure vessels and heat exchangers. The addition of tin gives added corrosion resistance.

     A highly ductile wrought nickel-free aluminum bronze with a nominal composition of CuAl7Fe2.5Sn. C61300 contains 2.5% iron, which facilitates added strength and acts as a grain refiner. C61300 also contains a small addition of tin, which aids corrosion resistance. The alloy is mainly produced in the form of plates for sea water applications and is also used in water condensing systems. It meets the requirements of ASTM B 150 C61300 (bars) and ASTM B 171 C61300 (plates).

Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
 

Typical Uses

General Characteristics

Applications

Good Electrical and Thermal Conductivity
Good Electroplating Ability
Good Corrosion Resistance
Good Cold Forming and Deep Drawing Qualities
Perfect Soldering and Welding
Excellent Against Stress Corrosion Cracking
Electric and Electronic Industry
Automotive Industry
Construction Industry
Circuit Breakers
Contact Springs
Lead Frames
Roofing  Jewelry
E.V. Components
 
Products List

Products List

Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

 

Certifications

CERTIFICATIONS

Quality is an integral part of our Business Principles. The quality policy guides us to deliver products and services that exceed the customers' expectations and meet all the standards. These principles have helped us to get recognition as a trusted vendor from customers around the world. Maxi Metal Products are trusted and chosen by customers all over the world. This trust is based upon our quality certification and our reputation for consistently delivering high-quality products.
 Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

Production flow
Production Flow
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

Anode casting wheel
The refined blister copper is poured into casting molds lined up side by side on the revolving circular table of a casting wheel and cast into anode plates for electrolytic refining. The anode plates are approximately 1m x 1m x 0.05m in size and weigh 380 kg per plate.

Refinery
Anode plates and stainless steel cathode plates are alternately set into the electrorefining cell, where a proper level of DC current is supplied. Dissolved copper from the anode is electrolytically deposited on the stainless steel cathode plate. After about 10 days of electrolysis, the cathode is lifted out and stripped from the stainless steel plate, resulting in the completion of refined copper (with a grade of 99.99%) as a final product.  The refined copper is shipped in stacked bulks, which are 1m in length and width and approximately 80kg in weight.
 
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

 

Packaging & Shipping
Packaging & Shipping
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware

 

Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
Company Profile

Who We Are?

Tianjin Zhongyantiancheng Steel Trading Co., Ltd

Tianjin Zhongyantiancheng Steel Trading Co., Ltd is the leader in the sale and distribution of aluminum, copper, copper alloys, brass, and bronze. We maintain huge inventories of aluminum, copper, brass, bronze, and specialty copper alloys. Our production and inventories consist of plates, coils, strips, foils, bars, tubes, rounds, hollows, rectangles, squares, hexagons, wires, and made-to-order shapes for customer-specific applications. We are the leading China alloy distributor of over one hundred different grades of aluminum and copper alloys in excess of 5000 metric tons.

Customers Visiting

Stress Corrosion Cracking Resistance 1000mm C61300 Bronze Plate for Marine Hardware
FAQ
FAQ
Q1:Can you send samples?
A: Of course, we can provide customers with samples and express shipping services all over the world.

Q2:What product information do I need to provide?
A: Please kindly provide the grade, width, thickness, surface treatment requirement should you have, and quantities you need to purchase.

Q3:It's my first time importing steel products, can you help me with it?
A: Sure, we have an agent to arrange the shipment, we will do it together with you.

Q4:How long does your delivery time take?
A: In general, our delivery time is within 7-15 days and may be longer if the quantity is extremely large or special circumstances occur.

Q5: How many countries have you already exported to?
A: We have exported to America, Canada, Brazil, Chile, Colombia, Russia, Ukraine, Thailand, Myanmar, Vietnam, India, Kenya, Ghana, Somalia, and other African countries. Our export experience is rich, we are familiar with different market demands, can help customers avoid a lot of trouble.

Q6:Can I go to your factory to visit?
A: Of course, we welcome customers from all over the world to visit our factory.

Q7:Does the product have a quality inspection before loading?
A: Of course, all our products are strictly tested for quality before packaging, and unqualified products will be destroyed and customers can appoint third parties to inspect the products before loading too.

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours